Search Tools

Concrete Maturity and Temperature–Time Factor

Report an issue

Relate concrete internal temperature history to a mix-specific calibrated relationship to obtain reference estimates of equivalent age and strength

Temperatures are interval-average internal concrete temperatures. Enter the datum temperature, activation energy and strength relationship from tests of the specific mix.

Strength is a reference estimate obtained by linear interpolation between calibration points. Continuous moist curing is assumed; suitability for formwork removal and similar decisions is not assessed.

What to calculate

Enter the actual reference temperature used for strength calibration, not an example value.

The Nurse–Saul datum temperature. Use a value below the calibration reference temperature.

Temperature–time historyRequired
RowElapsed time at interval end (h)Mean internal temperature during interval (°C)Actions
1
2

Paste 2 tab-separated columns into the leftmost field. Up to 240 rows.

Taking placement as 0 hours, enter each interval’s end time and mean internal concrete temperature in chronological order. Missing observations are not interpolated.

Calibrated strength data for the same mixRequired
RowEquivalent age (h)Compressive strength (MPa)Actions
1
2

Paste 2 tab-separated columns into the leftmost field. Up to 240 rows.

Enter at least 2 points of equivalent age in h → compressive strength in MPa, in ascending order, using the selected method and the same calibration reference temperature. Interpolation only; no extrapolation.

Results

Results update automatically when the required values are entered.

Method, applicability and sources

Calculation method

Nurse–Saul: M=Σ(Tᵢ−T₀)Δtᵢ (°C·h), and equivalent age tₑ=M/(Tᵣ−T₀) (h). Intervals with Tᵢ<T₀ are outside this calculation’s scope. Arrhenius: tₑ=Σexp[−(E/R){1/(Tᵢ+273.15)−1/(Tᵣ+273.15)}]Δtᵢ, with R=8.314 J/(mol·K); entered E is converted from kJ/mol to J/mol. Strength is found by linear interpolation between 2 adjacent calibrated equivalent-age/compressive-strength points for the same mix. Strength is not estimated outside the calibration range. Use interval-average temperatures for consecutive intervals starting at placement, 0h.

Worked example (hypothetical values)

Formula check example (not default inputs): with Nurse–Saul, T₀=−10°C, Tᵣ=20°C, mean temperature 10°C over 0–12h and 20°C over 12–24h give M=600°C·h and tₑ=20h. Calibration points (10h,10MPa) and (30h,30MPa) give an interpolated value of 20MPa.

Applicability and limitations

The same concrete mix, adequate moist curing, suitable temperature records, and conditions calibrated through strength testing. Does not transfer calibration to different mixes, correct for low-temperature cessation of strength development or freezing, interpolate missing observations, extrapolate strength beyond the calibration range, or determine long-term strength, formwork removal or construction suitability.

Method and sources

Method: Carino & Lew, The Maturity Method: From Theory to Application (NIST, 2001), Eq.(1)/(2); strength from user-supplied calibration points by linear interpolation. Data recorded: 2026-11-13.